Inclusions 
Cause Remedy
Improper sprues. Eliminate sharp corners in sprue system.
Crucible break down Replace crucible. Do not used old, disintegrating crucibles.
Dirty metal Do not use more than 50% recycled alloy and ensure it is clean.
Flasks overheated during burnout. Ensure maximum burnout temperature does not exceed 740ºC.
 
   